What causes corrosion?
Steel rusts when it comes into contact with factors such as moisture, oxygen and salt. This process is much faster at coastal facilities and in industrial areas. A paint system forms a barrier that isolates the steel from these factors; some primers also provide active protection.
1. Surface preparation: the foundation of the system
Even the best paint will deteriorate prematurely on a poorly prepared surface. Where possible, rust, scale and old paint should be removed by sandblasting; for maintenance work where sandblasting is not feasible, products suitable for mechanically cleaned surfaces should be used. The surface must be dry and free from oil and salt.
2. Primer: adhesion and corrosion prevention
The primer is the first coat that adheres directly to the steel and prevents corrosion. Epoxy primers offer good adhesion and chemical resistance. Examples:
- Penguard Primer – general-purpose epoxy primer
- Penguard Express ZP – fast-drying, zinc phosphate-containing epoxy
- Jotamastic 80 and Jotamastic 87 – surface-tolerant mastics for maintenance work where optimum surface preparation is not possible
3. Intermediate coat: thickness and barrier
The intermediate coat increases the system’s total film thickness, thereby hindering the passage of moisture and oxygen. In high-corrosion classes, the thickness of the intermediate coat directly determines the system’s service life. High-solids epoxies are used for this purpose.
4. Top coat: appearance and UV resistance
Epoxies chalk over time when exposed to sunlight; for this reason, polyurethane or acrylic products are preferred as the top coat in outdoor applications. Hardtop AX and Hardtop XP are examples of polyurethane top coats with high colour and gloss retention.
Example system approach
| Environment | Approach |
|---|---|
| Indoors, low humidity | An alkyd or single-coat epoxy system may be sufficient. |
| Industrial area, outdoor environment | Epoxy primer + epoxy intermediate coat + polyurethane top coat. |
| Coastal area, high corrosion | Epoxy system with a higher total thickness + polyurethane top coat; sandblasting where possible. |
The examples in the table are a general guide. Coat thicknesses and products must be determined in accordance with the project specifications and the products’ current technical data sheets.
Common mistakes
- Failure to observe inter-coat curing times
- Adjusting the mixing ratio by eye for two-component products
- Using the wrong thinner
- Handing over the work without measuring the dry film thickness
If you would like a system recommendation for your project, please provide us with details of the surface, environment and square metres.